Country of origin India

Compressive strength (dry) 133.2 MPa

Compressive strength (wet) 134.6 MPa

Water absorption   0.16%

Flexural strength   10.4 MPa

Abrasion resistance  27.0 Ha

Density  2,710 kg/m3

Modulus of Rupture  12.7 MPa


This Stone of the Month is supplied by Tab India of Jaipur, India. Technical details provide a frame of reference only. Because stone is a product of nature, testing to determine specific physical qualities should be repeated for each project. To submit your own Stone of the Month, send a high-resolution digital image, along with the relevant technical data, to adamsj@bnpmedia.com.